Photomicrograph of Krayn screen on an Autochrome plate.

Made:
c. 1909 in unknown place
Photomicrograph of Krayn screen on an Autochrome plate. Photomicrograph of Krayn screen on an Autochrome plate.

Creative Commons LicenseThis image is released under a CC BY-NC-SA 4.0 Licence

Buy this image as a print 

Buy

License this image for commercial use at Science and Society Picture Library

License

Creative Commons LicenseThis image is released under a CC BY-NC-SA 4.0 Licence

Buy this image as a print 

Buy

License this image for commercial use at Science and Society Picture Library

License

Science Museum Group
© The Board of Trustees of the Science Museum

Science Museum Group
© The Board of Trustees of the Science Museum

Photomicrograph of Krayn screen on an Autochrome plate.

The Krayn colour process was patented in 1904 by the German Robert Krayn, and was demonstrated by him in November 1907. Krayn stained very thin celluloid sheets red, green and blue, and cemented them interleaved to form a thick block from which thin slices were cut. Krayn was able to produce sheets of line screens up to 16 x 12 inches (40.6 x 30.5 cm) in size, with 175 colour lines to the inch (69 to the cm). Krayn’s process had a very limited commercial use, and in 1908 a finer screen, of 254 lines to the inch (100 to the cm) proved no more successful, the film being very prone to split along the lines of the cementing.

Details

Category:
Photographs
Object Number:
1928-256
Materials:
glass and paper (fibre product)
Measurements:
overall: 82 mm x 82 mm x 3 mm,
type:
photomicrographs
credit:
Gamble, C.W.